Blown film: bubble stability, gauge and strength

Choose a film resin for its behavior at your target output. Track the thin zone around the bubble and test the finished film in both directions.

Inflated tubular film above the extrusion die.

Choose each layer for the job it has to do

As the melt leaves the annular die, it has to withstand inflation and drawdown until it cools. Compare grades at the output your line needs. Record how the bubble behaves, how thickness varies around its circumference and how the finished film performs.

TargetMaterials to considerWhat to record
Stable bubbleFilm-grade LDPE, alone or in a blend. Its branched structure affects how the melt stretches.Die and bubble diameters, output, frost-line height and thickness profile.
Impact and puncture resistanceLLDPE or metallocene PE selected for the load the film will carry.Minimum thickness at the damaged spot, impact or puncture result and tear direction.
A tube that opens easilyA surface layer with an appropriate slip and antiblock package.Blocking after winding, friction on each side of the film and haze.

Is the thin band stationary or moving?

Mark one side of the bubble and track the thickness profile along the roll. If the thin area stays near one position on the die, check melt distribution and cooling around the die. If film width and thickness pulse together over time, compare the feed rate, pressure and changes in cooling.

A resin with different melt strength may help when bubble instability limits output. Record the working width, blow-up ratio, film thickness and the point at which the bubble becomes unstable. A photograph showing the whole bubble and the defect adds context to the melt flow rate.

What already goes into the roll?

Check the film grade’s additive package before changing the surface recipe. For example, LyondellBasell’s Lupolen 2427K is an LDPE film grade that contains erucamide and a mineral antiblock. For colored, printed or clear film, check pigment dispersion, ink adhesion or haze as appropriate.

If you return clean edge trim of known composition to the line, include its additives in the calculation. Record the area accepted at the specified minimum thickness, total resin consumption and stable production speed. For film strength and toughness, see the LLDPE film collection.

Why two films averaging 40 µm can fail differently

A thin band running the length of one roll can determine where a bag tears. Compare material cut from the band with material cut beside it, keeping the specimens in the same orientation.

  1. At the bubble. Mark the position of the thin band around the circumference when taking samples.
  2. At cutting. Keep a strip from that band in the machine direction (MD) and a matching strip from the adjacent area.
  3. At the filled bag. Record whether the tear starts in the same longitudinal band.

When a grade improves bubble stability, check that the benefit extends across the usable web and survives winding. Count savings from reducing gauge only on the length that passes converting and finished-package tests.

Two questions to settle before a film trial

Can the same LLDPE serve a monolayer film and a thin coextruded skin?

Check the function, thickness and share of the layer. A monolayer tube has to deliver all the required properties at once. A multilayer film can distribute those functions among its layers.

Why does a bag tear in only one direction?

Mark the starting point and the direction the tear travels relative to extrusion. Compare thickness and tear resistance in the machine and transverse directions (MD and TD) in the current film and a control film.

Blown-film grade directory

The collection contains 161 grade records. Open a family to see the grades and the properties listed in the Russian catalog. Some cards omit a test condition or unit. Check the grade data sheet before comparing those values.

LDPE · 53 grades
  • Sasol LFI2047A
    MFR: 4.7 g/10 min (ISO 1133, 190 °C / 2.16 kg) · Density: 0.920 g/cm³ (ISO 1183A) · Tensile strength: 27 / 15 MPa (ISO 527) · Processing: Blown film extrusion
  • Borouge FT7236
    MFR: 4.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.923 g/cm³ (ASTM D792) · Vicat softening temperature: 91 °C (ISO 306) · Processing: Film extrusion, Coextrusion
  • Borouge FT5230
    MFR: 0.75 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.923 g/cm³ (ASTM D792) · Processing: Film extrusion, Coextrusion, Lamination
  • Borouge FT6230
    MFR: 2.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.923 g/cm³ (ASTM D792) · Processing: Film extrusion, Coextrusion, Lamination, Foaming
  • Dow AGILITY 1500
    MFR: 0.15 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.920 g/cm³ (ASTM D792) · Impact: 210 g (ASTM D1709A, 51 µm film) · Processing: Blown film extrusion, Cast film extrusion
  • DOW LDPE 310E
    MFR: 0.75 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.923 g/cm³ (ASTM D792) · Impact: 170 g (ASTM D1709A, 50 µm blown film) · Processing: Blown film extrusion
  • DOW LDPE 312E
    MFR: 0.75 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.923 g/cm³ (ASTM D792) · Impact: 170 g (ASTM D1709A, 50 µm blown film) · Processing: Blown film extrusion
  • DOW LDPE 150E
    MFR: 0.3 g/10 min (ISO 1133, 190 °C / 2.16 kg) · Density: 0.921 g/cm³ (ASTM D792) · Impact: 430 g (ISO 7765-1) · Processing: Blown film extrusion
  • ExxonMobil LD 150BW — Film
    MFR: 0.75 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.923 g/cm³ (ASTM D1505) · Impact: 180 g (ASTM D1709A) · Processing: Blown film extrusion, Coextrusion, Lamination
  • ExxonMobil LD 100.BW
    MFR: 2.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.923 g/cm³ (ASTM D1505) · Impact: 110 g (ASTM D1709A) · Processing: Blown and cast film extrusion, Lamination, Compounding, Foaming
  • ExxonMobil LD 105.BR
    MFR: 2.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.923 g/cm³ (ASTM D1505) · Impact: 90 g (ASTM D1709A) · Processing: Blown and cast film extrusion, Lamination
  • ExxonMobil LD 129.DS
    MFR: 2.3 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.929 g/cm³ (ASTM D1505) · Impact: 70 g (ASTM D1709A) · Processing: Blown and cast film extrusion, Coextrusion, Embossing
  • ExxonMobil LD 165BW1
    Density: 0.922 g/cm³ (ASTM D1505) · Impact: 490 g (ASTM D1709A) · Processing: Blown film extrusion, Shrink film, Foaming, Profile extrusion
  • Formosa Plastics Formolene FL2202A
    MFR: 2.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.923 g/cm³ (ASTM D1505) · Impact: 80 g (ASTM D1709) · Processing: Blown film extrusion, Cast film
  • Formosa Plastics Formolene FL2202C
    MFR: 2.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.923 g/cm³ (ASTM D1505) · Impact: 80 g (ASTM D1709) · Processing: Blown film extrusion, Cast film
  • Formosa Plastics Formolene FR2375C
    MFR: 0.75 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.923 g/cm³ (ASTM D1505) · Impact: 180 g (ASTM D1709) · Processing: Blown film extrusion, Coextrusion
  • PETRONAS Chemicals C150Y
    MFR: 5 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.921 g/cm³ (ASTM D792) · Tensile strength: 15 / 26 MPa (ASTM D882) · Processing: Blown film extrusion
  • PETRONAS Chemicals N125Y
    MFR: 2.5 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.921 g/cm³ (ASTM D792) · Tensile strength: 15 / 29 MPa (ASTM D882) · Processing: Blown film extrusion
  • Lotte Chemical LDF260GG
    Density: 0.922 g/cm³ · Processing: Film extrusion
  • LyondellBasell Lupolen 2221D
    MFR: 0.25 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.922 g/cm³ (ASTM D1505, 23 °C) · Impact: 190 g (ASTM D1709, F50) · Processing: Blown film extrusion
  • LyondellBasell Lupolen 2227K
    MFR: 4.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.923 g/cm³ (ASTM D1505, 23 °C, material density) · Impact: 110 g (ASTM D1709, F50) · Processing: Blown film extrusion, Cast film, Compounding
  • LyondellBasell Lupolen 2420H
    MFR: 1.9 g/10 min (ISO 1133-1, 190 °C / 2.16 kg) · Density: 0.924 g/cm³ (ISO 1183-1) · Yield strength: 11 MPa (ISO 527-1, -2) · Processing: Blown film extrusion, Cast film
  • LyondellBasell Lupolen 2421H
    MFR: 1.9 g/10 min (ISO 1133-1, 190 °C / 2.16 kg) · Density: 0.924 g/cm³ (ISO 1183-1) · Yield strength: 11 MPa (ISO 527-1, -2) · Processing: Blown film extrusion, Cast film
  • LyondellBasell Lupolen 2426K
    MFR: 4.0 g/10 min (ISO 1133-1, 190 °C / 2.16 kg) · Density: 0.924 g/cm³ (ISO 1183-1) · Yield strength: 11 MPa (ISO 527-1, -2) · Processing: Blown film extrusion, Cast film
  • LyondellBasell Lupolen 2427F
    MFR: 0.75 g/10 min (ISO 1133, 190 °C / 2.16 kg) · Density: 0.924 g/cm³ (ISO 1183) · Yield strength: 11.0 MPa (ISO 527-1, -2) · Processing: Blown film extrusion
  • LyondellBasell Lupolen 2427H
    MFR: 1.9 g/10 min (ISO 1133, 190 °C / 2.16 kg) · Density: 0.924 g/cm³ (ISO 1183) · Yield strength: 11.0 MPa (ISO 527-1, -2) · Processing: Blown film extrusion, Cast film
  • LyondellBasell Purell PE 3020 D
    MFR: 0.30 g/10 min (ISO 1133, 190 °C / 2.16 kg) · Density: 0.927 g/cm³ (ISO 1183) · Yield strength: 13.0 MPa (ISO 527-1, -2, 23 °C) · Processing: Blow-fill-seal, Extrusion blow molding, Film extrusion, Injection molding
  • LyondellBasell LF2220PX
    MFR: 2.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.923 g/cm³ (ASTM D1505, 23 °C, material density) · Yield strength: 10 / 11 MPa (ASTM D882) · Processing: Blown film extrusion, Cast film
  • LyondellBasell Lupolen 2427K
    MFR: 4 g/10 min (ISO 1133, 190 °C / 2.16 kg) · Density: 0.924 g/cm³ (ISO 1183) · Strength: 19.0 / 16.0 MPa · Processing: Blown film extrusion, Cast film
  • QAPCO Lotrène FB3003
    MFR: Request test conditions · Density: 0.920 g/cm³ (ASTM D1505) · Impact: 175 g (ASTM D1709) · Processing: Film extrusion
  • QAPCO Lotrène FB5026
    MFR: Request test conditions · Density: 0.920 g/cm³ (ASTM D1505) · Impact: 175 g (ASTM D1709) · Processing: Film extrusion
  • QAPCO Lotrène FD0270
    MFR: Request test conditions · Density: 0.923 g/cm³ (ASTM D792) · Impact: 85 g (ASTM D1709) · Processing: Film extrusion, Lamination
  • QAPCO Lotrène FD0274
    MFR: Request test conditions · Density: 0.923 g/cm³ (ASTM D1505) · Impact: 110 g (ASTM D1709) · Processing: Film extrusion, Cast film
  • QAPCO Lotrène FD0374
    MFR: Request test conditions · Density: 0.923 g/cm³ (ASTM D1505) · Impact: 100 g (ASTM D1709) · Processing: Film extrusion, Cast film
  • QAPCO Lotrène FD0474
    MFR: Request test conditions · Density: 0.923 g/cm³ (ASTM D1505) · Impact: 90 g (ASTM D1709) · Processing: Film extrusion, Cast film
  • QAPCO Lotrène FE3000
    MFR: Request test conditions · Density: 0.923 g/cm³ (ASTM D792) · Impact: 150 g (ASTM D1709) · Processing: Film extrusion
  • QAPCO Lotrène FE8000
    MFR: Request test conditions · Density: 0.923 g/cm³ (ASTM D1505) · Impact: 150 g (ASTM D1709) · Processing: Film extrusion
  • QAPCO Lotrène FE8004
    MFR: Request test conditions · Density: 0.923 g/cm³ (ASTM D792) · Impact: 110 g (ASTM D1709) · Processing: Film extrusion, Lamination
  • SABIC HP0322N
    MFR: 0.33 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.922 g/cm³ (ASTM D1505) · Impact: 4 g/µm (ASTM D1709) · Processing: Blown film extrusion
  • SABIC HP0723JN
    MFR: 0.75 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.923 g/cm³ (ASTM D792) · Tensile strength: 25.0 MPa (ASTM D882) · Processing: Blown film extrusion
  • SABIC HP2022JN
    MFR: 2.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.922 g/cm³ (ASTM D1505) · Impact: 2 g/µm (ASTM D1709) · Processing: Blown film extrusion
  • SABIC HP2023JN
    MFR: 2.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.923 g/cm³ (ASTM D1505) · Impact: 2 g/µm (ASTM D1709) · Processing: Blown film extrusion
  • SABIC HP2025JN
    MFR: 2.00 g/10 min (ISO 1133, 190 °C / 2.16 kg) · Density: 0.925 g/cm³ (ASTM D792) · Impact: 110 g (ASTM D1709) · Processing: Blown film extrusion
  • SABIC HP4024WN
    MFR: 4.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.923 g/cm³ (ASTM D1505) · Impact: 2 g/µm (ASTM D1709) · Processing: Blown film extrusion, Compounding
  • SABIC HP4025ZN
    MFR: 3.5 g/10 min (ISO 1133, 190 °C / 2.16 kg) · Density: 0.923 g/cm³ (ASTM D792) · Impact: 2 g/µm (ASTM D1709) · Processing: Blown film extrusion
  • Sasol LF2207F
    MFR: 0.75 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.922 g/cm³ (ASTM D1505) · Tensile strength: 22 / 20 MPa (ASTM D882) · Processing: Blown film extrusion
  • Sasol LF2220M
    MFR: 2.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.922 g/cm³ (ASTM D1505) · Tensile strength: 21 / 17 MPa (ASTM D882) · Processing: Blown film extrusion
  • Saudi Tasnee 1925AS
    MFR: 1.90 g/10 min (ISO 1133, 190 °C / 2.16 kg) · Density: 0.925 g/cm³ (ISO 1183) · Tensile strength: 26 / 18 MPa MD / TD (ISO 527-1, -3) · Processing: Film extrusion
  • Tasnee 4025AS
    MFR: 4.0 g/10 min (ISO 1133, 190 °C / 2.16 kg) · Density: 0.925 g/cm³ (ISO 1183) · Tensile strength: 22 / 15 MPa MD / TD (ISO 527-1, -3) · Processing: Film extrusion
  • PTT Global Chemical LD2420H
    MFR: 1.9 g/10 min · Density: 0.924 g/cm³ · Processing: Film extrusion
  • PTT Global Chemical LD2426H
    MFR: 1.9 g/10 min · Density: 0.924 g/cm³ · Processing: Film extrusion
  • PTT Global Chemical PTT-LD2420D
    MFR: 0.27 g/10 min · Density: 0.922 g/cm³ · Processing: Film extrusion, Blow molding
  • Braskem LDF2023S1
    MFR: Request test conditions · Density: 0.920 g/cm³ (ASTM D792) · Impact: 110 (ASTM D 1709/A) · Processing: Blown film extrusion
LLDPE · 65 grades
  • Aramco LLDPE F2122BS
    MFR: 2.2 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.921 g/cm³ (ASTM D792, method A) · Tensile strength: 35 / 30 MPa (ASTM D882) · Processing: Blown film extrusion
  • Borouge Anbiq FM1810
    MFR: 1.1 g/10 min (ISO 1133, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ISO 1183) · Tensile strength: 50/40 MPa (ISO 527-3, MD / TD) · Processing: Film extrusion, Coextrusion, Lamination, Modification
  • Borouge Borstar FB1370
    MFR: 0.12 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.938 g/cm³ (ASTM D792) · Processing: Wide film extrusion, Coextrusion, Geomembranes
  • DOWLEX 2645
    MFR: 0.85 g/10 min (ISO 1133, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D792) · Impact: 480 g (ISO 7765-1/A, 50 µm film) · Processing: Blown film extrusion
  • DOWLEX 2645.11G
    MFR: 0.90 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.921 g/cm³ (ASTM D792) · Tensile strength at break (MD): 48.8 MPa (ASTM D882, Film 50.8 µm, BUR 2.5, 2009-05-20, MD) · Processing: Blown film extrusion
  • DOWLEX 2045.11G
    MFR: 1.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.922 g/cm³ (ASTM D792) · Processing: Blown film extrusion
  • DOWLEX 2045G
    MFR: 1.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.920 g/cm³ (ASTM D792) · Tensile strength at break (MD): 47.4 MPa (ASTM D882, Film 25 µm, BUR 2.5, 2013-01-18, MD) · Processing: Blown film extrusion
  • DOWLEX 2645G
    MFR: 0.90 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.919 g/cm³ (ASTM D792) · Impact: 300 g (ASTM D1709A, 51 µm film) · Processing: Blown film extrusion
  • Dow CEFOR 1220P
    MFR: 2.0 g/10 min (ISO 1133, 190 °C / 2.16 kg) · Density: 0.919 g/cm³ (ASTM D792) · Impact: 140 g (ASTM D1709A, 38 µm film) · Processing: Blown film extrusion
  • EQUATE EFDC7050
    MFR: Request test conditions · Impact: 85 (ASTM D 1709A) · Processing: Film extrusion, Blow molding, Fiber forming
  • ExxonMobil LL 1001AV
    MFR: 1.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D792) · Impact: 90 g (ASTM D1709A) · Processing: Blown film extrusion, Coextrusion, Blending with LDPE
  • ExxonMobil LL 1002BU
    MFR: 2.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D792) · Impact: <60 g (ASTM D1709A) · Processing: Blown film extrusion, Flat film extrusion, Lamination
  • ExxonMobil LL 1002YB
    MFR: 2.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D792) · Tensile strength at break (MD): 60 MPa (ASTM D882, Film 20.3 µm, 06/01/2013, MD) · Processing: Cast and blown film extrusion, Stretch film
  • ExxonMobil Exceed 1018 Series
    MFR: 1.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D792) · Impact: 550 g (ASTM D1709A) · Processing: Blown film extrusion, Multilayer film, Lamination
  • ExxonMobil Exceed 1018FA
    MFR: 1.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D4703 / D1505) · Tensile strength (MD): 50 MPa (ASTM D882) · Processing: Single- and multilayer blown film extrusion
  • ExxonMobil Exceed 1018MK
    MFR: 1.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D1505) · Impact: 460 g (ASTM D1709A) · Processing: Blown film extrusion, Multilayer film, Lamination
  • ExxonMobil Exceed 1518MM
    MFR: 1.5 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D1505) · Impact: 540 g (ASTM D1709A) · Processing: Blown film extrusion, Multilayer packaging film
  • ExxonMobil Enable 2010 Series (2010ME / 2010PA)
    MFR: 1.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.920 g/cm³ (ASTM D792) · Impact: 180 g (ASTM D1709A) · Processing: Blown and cast film extrusion, Stretch film, Heat shrinking, Lamination
  • ExxonMobil Exceed 3518CB
    MFR: 3.5 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D792) · Impact: 140 g (ASTM D1709A) · Processing: Single- and multilayer cast film extrusion, Stretch film
  • ExxonMobil Exceed 3518PA
    MFR: 3.5 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D792) · Impact: 140 g (ASTM D1709A) · Processing: Single- and multilayer cast film extrusion, Stretch film
  • ExxonMobil LL 1002 Series (X75 / 1002.09 / 1002.80)
    MFR: 2.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D1505) · Impact: 70 g (ASTM D1709A) · Processing: Blown and cast film extrusion, Compounding of version 1002.09
  • ExxonMobil LL 1002xBU
    MFR: 2.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D1505) · Impact: <60 g (ASTM D1709A) · Processing: Blown film extrusion, Flat film extrusion, Lamination
  • Formosa Plastics L42009F
    MFR: 0.95 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.919 g/cm³ (ASTM D1505) · Tensile strength: 5100 / 3225 psi (ASTM D882) · Processing: Blown film extrusion, Coextrusion
  • Formosa Plastics LB1810B
    Processing: Film extrusion
  • Formosa Plastics LB1810E2
    Processing: Film extrusion
  • Hanwha TotalEnergies 3224
    MFR: 2.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.920 g/cm³ (ASTM D1505) · Tensile strength: 185 kg/cm² (ASTM D638) · Processing: Blown film extrusion
  • Hanwha TotalEnergies LLD3304
    MFR: 1.1 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.923 g/cm³ (ASTM D1505) · Yield strength: 130 / 120 kg/cm² (ASTM D882, MD / TD, 0.025 mm film) · Processing: Blown film extrusion
  • Luqing LEF35BN
    MFR: 2.0 g/10 min · Density: 0.92 g/cm³ · Strength: 9.65 MPa · Processing: Film extrusion, Monofilament extrusion
  • Chevron Phillips Marlex D139
    MFR: 1.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D1505) · Processing: Film extrusion, Coextrusion
  • Chevron Phillips Marlex D139FK
    MFR: 1.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D1505) · Processing: Film extrusion, Coextrusion
  • Chevron Phillips Marlex D143FK
    MFR: 1.4 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.916 g/cm³ (ASTM D1505) · Processing: Film extrusion, Coextrusion
  • NOVAPOL PF-0218B
    Density: 0.918 g/cm³ (ASTM D792) · Tensile strength: 32 / 25 MPa (ASTM D882) · Processing: Blown film extrusion
  • OQ Luban DFDA-7059
    MFR: 2 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D792) · Yield strength: 7.4 / 6.5 MPa (ASTM D882) · Processing: Cast film, Blown film extrusion
  • OQ Luban DFDA-7042
    MFR: 2 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D792) · Yield strength: 11 / 10 MPa (ASTM D882) · Processing: Blown film extrusion, Cast film
  • OQ Luban DFDC-7080
    MFR: 1 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D792) · Tensile strength: 57 / 38 MPa (ASTM D882) · Processing: Blown film extrusion, Cast film, Irrigation tubing extrusion
  • PTT Global Chemical LL7410D
    Density: 0.921 g/cm³ · Processing: Film extrusion
  • PTT Global Chemical InnoPlus LL7420A
    MFR: 2.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D792) · Tensile strength: 31 / 23 MPa (ASTM D882) · Processing: Blown film extrusion, Cast film
  • PTT Global Chemical LL7420D
    Density: 0.921 g/cm³ · Processing: Film extrusion
  • Qatofin Lotrène Q1018 Series
    MFR: 1.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D792) · Impact: 150 g (ASTM D1709) · Processing: Film extrusion, Coextrusion
  • Qatofin Lotrène Q2018 Series
    MFR: 2.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D792) · Impact: 130 g (ASTM D1709) · Processing: Film extrusion, Cast film, Coextrusion
  • SABIC 118NJ
    MFR: 1 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D1505) · Strength: 40 MPa · Processing: Blown film extrusion
  • SABIC 118WJ
    MFR: 1 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D1505) · Impact: 145 g/µm (ASTM D1709, source gives 145 g/µm; confirm that unit before using the figure) · Processing: Blown film extrusion
  • SABIC 118WSJ
    MFR: 1 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D1505) · Impact: 145 g/µm (ASTM D1709) · Processing: Blown film extrusion
  • SABIC 119NJ
    MFR: 1 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.919 g/cm³ (ASTM D792) · Impact: 100 g (ASTM D1709) · Processing: Blown film extrusion
  • SABIC 119ZJ
    MFR: 2.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D792) · Impact: 144 g (ASTM D1709) · Processing: Blown film extrusion
  • SABIC 122NJ
    MFR: 1.1 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.921 g/cm³ (ASTM D792) · Impact: 115 g (ASTM D1709) · Processing: Blown film extrusion
  • SABIC 218BJ
    MFR: 2.0 g/10 min (ISO 1133, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D1505) · Vicat softening temperature: 96 °C (ISO 306) · Processing: Blown film extrusion, Cast film
  • SABIC 218NJ
    MFR: 2 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D1505) · Impact: 85 g/µm (ASTM D1709) · Processing: Blown film extrusion
  • SABIC 218WJ
    MFR: 2 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D1505) · Vicat softening temperature: 98 °C (ASTM D1525) · Processing: Blown film extrusion
  • SABIC 222WJ
    MFR: 2.2 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.921 g/cm³ (ASTM D792) · Tensile strength at break (MD): 35 MPa (ASTM D882, Film 30 µm, BUR 2, 20211203, MD) · Processing: Blown film extrusion
  • SABIC 6821NJ
    MFR: 0.8 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.921 g/cm³ (ASTM D1505) · Impact: 150 g/µm (ASTM D1709) · Processing: Blown film extrusion
  • SABIC 219ZJ
    MFR: 2.0 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (ASTM D792) · Impact: 144 g (ASTM D1709) · Processing: Blown film extrusion
  • Sibur 20211FE
    MFR: 2 g/10 min · Density: 0.921 g/cm³ · Processing: Film extrusion
  • Sibur LL20200FE
    MFR: 2 g/10 min (ISO 1133-1, 190 °C / 2.16 kg) · Density: 0.920 g/cm³ (ISO 1183) · Tensile strength: 36 / 30 MPa (ISO 527-1) · Processing: Blown film extrusion, Cast film, Coextrusion, Blending with LDPE
  • Sinopec DFDA7042
    Processing: Film extrusion, Pipe extrusion, Tape forming
  • Sumitomo Chemical / Petro Rabigh FS253S
    MFR: 2.2 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.921 g/cm³ (ASTM D792-A) · Tensile strength: 35 / 30 MPa (ASTM D882) · Processing: Blown film extrusion
  • China Coal Shaanxi Yulin Energy Chemical 7042
    MFR: Request test conditions · Density: 0.921 g/cm³ (GB/T 1033.2) · Yield strength: 9.53 MPa (GB/T 1040.2) · Processing: Blown film extrusion
  • SABIC 920NT
    MFR: 0.85 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.920 g/cm³ (ASTM D1505) · Strength: 10 MPa · Processing: Blown film extrusion
  • SABIC 222WT
    MFR: 1.9 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.922 g/cm³ (ASTM D1505) · Strength: 10 MPa · Processing: Blown film extrusion
  • Yulong LLD-7042
    MFR: 2 g/10 min (GB/T 3682.1-2018, 190 °C / 2.16 kg) · Density: 0.919 g/cm³ (GB/T 1033.2-2010) · Yield strength: 8 MPa (GB/T 1040.2-2022) · Processing: Blown film extrusion, Cast film
  • Yulong LLD-7047
    MFR: 1 g/10 min (GB/T 3682.1-2018, 190 °C / 2.16 kg) · Density: 0.919 g/cm³ (GB/T 1033.2-2010) · Tensile strength: ≥12 MPa (GB/T 1040.2-2022) · Processing: Blown film extrusion, Cast film
  • Yulong LLD-7050
    MFR: 2 g/10 min (GB/T 3682.1-2018, 190 °C / 2.16 kg) · Density: 0.919 g/cm³ (GB/T 1033.2-2010) · Yield strength: ≥8 MPa (GB/T 1040.2-2022) · Processing: Blown film extrusion, Cast film
  • Yulong mPE-1018
    MFR: 1 g/10 min (GB/T 3682.1-2018, 190 °C / 2.16 kg) · Density: 0.918 g/cm³ (GB/T 1033.2-2010) · Tensile strength: 15 MPa (GB/T 1040.2-2022) · Processing: Film extrusion
  • Luqing LEF-34
    MFR: 1.0 g/10 min · Density: 0.9189 g/cm³ · Strength: 10.8 MPa · Processing: Film extrusion, Monofilament extrusion
  • Braskem LL4405S
    Density: 0.922 g/cm³ · Processing: Blown film extrusion
HDPE · 24 grades
  • EQUATE 6888
    Density: 0.952 g/cm³ (ASTM D 1505) · Impact: 150 (ASTM D 1709 A) · Processing: Film extrusion, Blow molding, Fiber forming
  • ExxonMobil HD 7960.13
    MFR: 0.060 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.952 g/cm³ (ASTM D1505) · Yield strength: 37 MPa (ASTM D882) · Processing: Blown film extrusion
  • ExxonMobil HTA 001HD5
    MFR: 0.32 g/10 min (ASTM D1238, 190 °C / 5 kg) · Density: 0.952 g/cm³ (ASTM D1505) · Yield strength: 41 MPa (ASTM D882) · Processing: Blown film extrusion
  • ExxonMobil HTA 108
    MFR: 0.70 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.961 g/cm³ (ASTM D1505) · Impact: <30 g (ASTM D1709A) · Processing: Blown film extrusion, Coextrusion, Blending with PE
  • Formosa Plastics E924
    MFR: 0.04 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.949 g/cm³ (ASTM D1505) · Tensile strength: 9000/4100 psi (ASTM D882, MD / TD, 0.50 mil blown film) · Processing: Blown film extrusion
  • Formosa Plastics HDPE9000
    MFR: 0.07 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.950 g/cm³ (ASTM D1505) · Yield strength: 260 kg/cm² (ASTM D638) · Processing: Blown film extrusion
  • GS Caltex TR-144
    Tensile strength: >26 MPa (ASTM D882) · Processing: Film extrusion
  • Lotte Chemical FL7000
    MFR: Request test conditions · Density: 0.956 g/cm³ (ASTM D1505) · Yield strength: 250 kgf/cm² (ASTM D638) · Processing: Blown film extrusion
  • Saudi Polymers Marlex HHM TR-144
    MFR: 0.18 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.946 g/cm³ (ASTM D1505) · Flexural modulus: 1150 MPa (ASTM D790) · Processing: Film extrusion
  • Chevron Phillips Marlex TRB-115
    MFR: 0.06 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.950 g/cm³ (ASTM D1505) · Processing: Film extrusion
  • Q-Chem Lotrène Q TR-144
    MFR: 0.18 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.946 g/cm³ (ASTM D1505) · Flexural modulus: 1150 MPa (ASTM D790) · Processing: Film extrusion
  • SABIC FI0750
    MFR: 0.22 g/10 min (ISO 1133, 190 °C / 5 kg) · Density: 0.950 g/cm³ (ASTM D1505, converted from 950 kg/m³) · Tensile strength: 50 MPa (ISO 527-3, 20 µm blown film) · Processing: Film extrusion
  • SABIC FI0851P
    MFR: 0.05 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.951 g/cm³ (ASTM D792) · Processing: Blown film extrusion
  • SABIC FJ00952
    MFR: 0.05 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.952 g/cm³ (ASTM D1505, converted from 952 kg/m³) · Tensile strength: 60 MPa (ASTM D882, 15 µm film) · Processing: Film extrusion
  • SABIC FJ01552
    MFR: 0.15 g/10 min (ISO 1133, 190 °C / 2.16 kg) · Density: 0.952 g/cm³ (ASTM D1505, converted from 952 kg/m³) · Tensile strength: 55 MPa (ASTM D882, 15 µm film) · Processing: Film extrusion
  • SK HDPE 8300
    Density: 0.963 g/cm³ · Processing: Film extrusion
  • Sinochem HD55110
    MFR: 10 g/10 min (GB/T 3682.1, 190 °C / 21.6 kg) · Density: 0.955 g/cm³ (GB/T 1033.2, 23 °C) · Yield strength: ≥20 MPa (GB/T 1040.2) · Processing: Blown film extrusion
  • Sumitomo Chemical F0554
    MFR: 0.05 g/10 min (190 °C / 2.16 kg) · Density: 0.951 g/cm³ · Strength: 35 MPa · Processing: Blown film extrusion
  • Tricon Energy HDF05952
    MFR: 0.06 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.952 g/cm³ (ASTM D1505, 23 °C) · Tensile strength: 76 MPa (ASTM D882) · Processing: Blown film extrusion
  • Yulong HD-6098
    MFR: Request test conditions · Density: 0.950 g/cm³ (GB/T 1033.2-2010) · Yield strength: ≥20 MPa (GB/T 1040.2-2022) · Processing: Blown film extrusion
  • Yulong HD-7000F
    MFR: Request test conditions · Density: 0.951 g/cm³ (GB/T 1033.2-2010) · Yield strength: ≥20 MPa (GB/T 1040.2-2022) · Processing: Blown film extrusion
  • Yulong HD-TR144
    MFR: Request test conditions · Density: 0.945 g/cm³ (GB/T 1033.2-2010) · Yield strength: 21.5 MPa (GB/T 1040.2-2022) · Processing: Blown film extrusion
  • Luqing ACP7000F
    MFR: Request test conditions · Density: 0.9523 g/cm³ (GB/T 1033.2-2010) · Yield strength: 27.0 MPa (GB/T 1040.2-2022) · Processing: Blown film extrusion
  • Braskem HDF8000
    MFR: Request test conditions · Density: 0.949 g/cm³ (ASTM D 792) · Impact: 416 (ASTM D1709/A) · Processing: Blown film extrusion
MDPE · 3 grades
  • Chevron Phillips Marlex HHM TR-130
    Melt index: 0.3 g/10 min · Density: 0.937 g/cm³ (ASTM D1505) · Processing: Film extrusion
  • Q-Chem Marlex HHM TR-131
    Melt index: 0.2 g/10 min · Density: 0.938 g/cm³ (ASTM D1505) · Processing: Film extrusion
  • Borouge Borstar FB1350
    MFR: 0.15 g/10 min (ASTM D1238, 190 °C / 2.16 kg) · Density: 0.935 g/cm³ · Strength: 65 MPa · Processing: Film extrusion, Coextrusion, Lamination
PP · 13 grades
  • Borealis RB707CF
    MFR: 1.5 g/10 min (ISO 1133-1, 230 °C / 2.16 kg) · Notched Charpy impact: 25 kJ/m² (ISO 179-1, 23 °C) · Processing: Non-oriented film extrusion, Coextrusion, Lamination
  • Formosa Plastics F1611
    MFR: 10.5 g/10 min (ASTM D-1238, 230 °C / 2.16 kg) · Density: 0.900 g/cm³ (ASTM D-792 / ISO 1183, 23 °C/23 °C) · Yield strength: 35 MPa (ASTM D-638 / ISO 527, 23 °C) · Processing: Blown film extrusion
  • Grand Resource PPH-GF10S
    MFR: 10.0 g/10 min (GB/T 3682.1-2018, 230 °C / 2.16 kg) · Flexural modulus: ≥1300 MPa (GB/T 9341-2008) · Processing: Film extrusion, Blown film
  • Lotte Chemical PD943
    MFR: 11 g/10 min · Density: 0.9 g/cm³ · Processing: Film extrusion
  • LyondellBasell RP270G
    MFR: 1.8 g/10 min (ISO 1133-1, 230 °C / 2.16 kg) · Density: 0.90 g/cm³ (ISO 1183-1) · Yield strength: 25 MPa (ISO 527-1) · Processing: Blow-fill-seal, Blow molding, Film extrusion, Injection molding
  • OQ HP4128N
    MFR: 10.5 g/10 min (ASTM D1238, 230 °C / 2.16 kg) · Density: 0.90 g/cm³ (ASTM D792) · Yield strength: 35 MPa (ASTM D638) · Processing: Cast film extrusion, Water-quenched film extrusion
  • OQ RP4202M
    MFR: 6 g/10 min (ISO 1133, 230 °C / 2.16 kg) · Density: 0.900 g/cm³ (ASTM D1505) · Yield strength: 27 MPa (ISO 527-2) · Processing: Cast film extrusion, Water-quenched film extrusion
  • Qingdao Jinneng HP520J
    MFR: Request test conditions · Yield strength: ≥33 MPa (GB/T 1040.2) · Processing: Film extrusion
  • SABIC PP 520L
    MFR: 10 g/10 min (ASTM D1238, 230 °C / 2.16 kg) · Density: 0.905 g/cm³ (ASTM D792) · Flexural modulus: 1600 MPa (ASTM D790A) · Processing: Film extrusion
  • SCG Chemicals P600F
    Density: 0.910 g/cm³ · HDT / Vicat: 155 °C · Processing: Film extrusion
  • SCG Chemicals P601F
    Density: 0.910 g/cm³ · Processing: Film extrusion
  • Chambroad F03D
    MFR: Request test conditions · Yield strength: 31.5 MPa (GB/T 1040) · Processing: Film extrusion, Biaxial orientation, Cast film
  • PetroChina Guangdong L5E89
    MFR: Request test conditions · Yield strength: ≥29.0 (GB/T 1040.2) · Processing: Extrusion, Film extrusion
PA6 · 2 grades
Copolyamide · 1 grade